Thought I'd post this after Calv asked me if there was anything he could do with some brittle FP:-
Using an electric skilled; Put the FP on a Teflon sheet in a dry skillet and heat for 2-3 minutes after it has softened, it reconditions the plastic and when it is cool (leave on the side to cool naturally), it is pliable and bendy just as it should be. The only thing we don't know, is how long the reconditioning lasts for!
HTH